2) Started sanding with a DA (dual action sander) with a 36 grit paper.
3) Started working on the dent on the front edge of the hood. We banged it out with a hammer from the underside and then filled what was left with filler.
4) Sanded hood again. This time with 80 grit paper.
6) Applied 4 coats of ppg primer.
7) Applied one coat of guide coat.